Electroless Nickel:

  • High phosphorus ( 10 to 12 % )
  • Medium Phosphorus ( 8 to 10 %)
  • Low Phosphorus ( 3 to 5 % )
  • Alkaline
 Process
P Content
 Products
Features
Applications

High Phosphorus

10 - 12 %

- Marshal EN 825
- Marshal EN 423
- Marshal EN 9304

- Semibright deposit
- Offers high corrosion resistance, 1000 Hrs Salt Spray
- Non Magnetic
Amorphous

- Oil/Petroleum Industrial vales and other components.
- All components exposed to atmosphere
- Computers
- Printed Circuit Boards

Medium Phosphorus

8 - 10 %

 - Marshal EN 814
- Marshal EN 855

- Bright Lustorus deposits
- Higher plating speed ( > 15 microns/ hr )
- Higher Metal Turn overs
- Medium Corrosion resistance
( 100 Hrs Salt Spray )

- Printers and Type writers
- Computer/ business machines
- Industrial components

Low Phosphorus

3 - 5 %

 - Marshal EN 826

- Bright Deposit
- Higher Hardness value
( 50 R C )
- Ductile Deposit
- Suitable for Wire Bonding / Soldering in case of PCBs

- Dies 
- Printed Circuit Boards
- Industrial Components where high hardness is required

Alkaline

< 3 %

 - Marshal EN 804

- Room temperature electroelss nickel
- Stable alkaline formulation
- Uniform coverage

- ABS Plastic plating undercoat

Alkaline

< 3 %

 - Marshal EN - Al 105

- Room temperature electroelss nickel
- Stable

- Overcoat after Zincate layer on Aluminum surface as a sacrificial bath